Abstract
Improving the deformation behaviour of titanium alloys at intermediate temperatures is crucial for cost and energy savings in forming processes. In this context, the modification of the microstructure prior to forming is of great importance. Here we show how the deformability of α-β titanium sheets at 500 °C can be significantly increased via a tailored pre-heating procedure in the range of 750–950 °C, with an optimal range of 790–850 °C. Depending on the pre-heating temperature and the subsequent cooling conditions, major changes in hardening behaviour were achieved, resulting in increased elongation and/or tensile strength. Based on these results, an elongated cup was deep drawn at 500 °C after the pre-heating treatment, without relying on superplastic forming. Our results highlight the potential to develop an economic production process for thin-walled titanium components via deep drawing at intermediate temperatures.
| Original language | English |
|---|---|
| Article number | 115509 |
| Number of pages | 10 |
| Journal | Materials & Design |
| Volume | 262 |
| DOIs | |
| Publication status | Published - 23 Jan 2026 |
UN SDGs
This output contributes to the following UN Sustainable Development Goals (SDGs)
-
SDG 9 Industry, Innovation, and Infrastructure
Research Field
- Advanced Forming Processes and Components
Keywords
- Forming
- α-β alloys
- Titanium sheet
- deep drawing
- strain hardening