Surface Analysis of Biodegradable Mg-Alloys after Immersion in Simulated Body Fluid

  • Darja Steiner Petrovič
  • , Djordje Mandrino
  • , Bozidar Sarler
  • , Jelena Horky
  • , Andrea Ojdanic
  • , Michael Zehetbauer
  • , Dmytro Orlov
    • University of Vienna
    • Lund University

    Research output: Contribution to journalArticlepeer-review

    Original languageEnglish
    Pages (from-to)1740
    Number of pages1
    JournalMaterials
    Volume13
    DOIs
    Publication statusPublished - 2020