Skip to main navigation Skip to search Skip to main content

Surface Analysis of Different Boundary Layers on Steel Discs Formed in a Lubricated Tribocontact During Laboratory Test Compared with Field Application

  • Astrid Stadler
  • , Josef Brenner
  • , Andreas Pauschitz
  • , Josef Wendrinsky
  • , Andreas Schindel
  • , Gerhard Nauer

    Research output: Contribution to journalArticlepeer-review

    Original languageEnglish
    Pages (from-to)1527-1535
    Number of pages9
    JournalAnalytical and Bioanalytical Chemistry
    Publication statusPublished - 2008

    Research Field

    • Not defined

    Cite this